A drop of water is placed on.
How to test for contaminants on concrete floor.
Therefore it s advisable to have a floor tested for moisture content prior to installing flooring or moisture barriers.
Surface needs to sanded using a diamond grinder.
Sixty to seventy two hours later the dish is weighed again.
To complete a penetration resistance test a device drives a small pin or probe into the surface of the concrete.
Ble contaminants include concrete surface hardeners curing agents form release agents waterproofing compounds and oil or grease.
Data is significantly affected by surface conditions as well as the type of form.
As noted acids from a variety of sources as well as mildew also can cause contamination.
This document provides information about sewage backup hazards testing inspection and cleanup remediation in residential and commercial buildings.
Remove all loose or un bonded coating.
Except for the contamination the concrete is in excellent condition.
Surface was contaminated by water humidity oil dust or grease.
While this may be an inconvenience it isn t a death sentence.
Subsequently the floor surface must be properly prepared by milling shot blasting etc.
The building is being converted to a store and the owner wants to paint the floor.
The surveyor may not see any evidence of possible damage caused by sulphate action but will still ask for a test to be carried out due to the age of the property.
Improper mixing methods.
The force used to penetrate the surface and the depth of the hole is correlated to the strength of the in place concrete.
Concrete slabs and floors can be excellent subfloor surfaces for tile and other floor coverings but too much moisture in the concrete can cause problems with flooring installations.
Sulphate floor tests are usually requested by surveyors when a property is being sold or remortgaged etc.
Coating was not mixed at proper ratio or for 3 minutes at minimum.
Sewage backups contamination response.
A plastic sheet is taped to the concrete surface and left in place for 16 hours or more then removed and inspected for condensation.
One is a water drop test.
Relatively easy to use and can be done directly onsite.
A dish containing calcium chloride is weighed then placed on the concrete surface and sealed under a dome.
Although the request for a test is at the discretion of the individual surveyor.
If the concrete core test results reveal your concrete is contaminated with hydrocarbons the slab will need to be cleaned and sealed to prevent these contaminates from causing flooring failures.
The surface contaminants only to ex continued q a building has been used as a car garage for years and the concrete floor has been well contaminated with oil grease antifreeze etc.
Vacuum to remove all dust.
Fd clean is then spread on the floor and rubbed meticulously with a hard wire brush in order to penetrate the substrate pores and emulsify the oil or fat.