It can fill large holes.
How to repair spalling floor in waffle slab.
Apply two coats of anti rust paint to the steel bars.
It works extremely well.
And not curing the concrete.
Clean the prepared area.
I m using ardex cd con.
You want to give your repair something stable and solid to adhere to so don t skimp.
If the damage is greater than 1 3 of the depth steel bars may need to be installed and a full depth restoration may be required.
Sprinkling the surface of the concrete with water to extend finishing time.
Sweep and vacuum the damaged area until all of the loose pieces are gone.
It s easily applied to spalling that covers large areas.
When the spalling damage is shallower than 1 3 of the concrete s thickness the concrete usually can receive a surface repair.
It can be trowelled out smoothly over pits.
Expert advice on why spalled concrete occurs and how to fix it.
Scrape and clean the exposed steel bars and use a wire brush to remove the rust.
Step 3 choosing epoxy for concrete spalling repair.
It is the go to method for floor coating contractors.
Indeed you can use resurfacer to revive just about any worn out.
Common mistakes include adding too much water to the mix to make it easier to pour.
Tips on how to repair spalled concrete.
Remove all of the loose material.
Remove the concrete at the spalled areas to expose the corroded steel bars.
Believe it or not that s all it takes to deal with spalling on your driveway or your patio walkway or garage floor slab.
The basic steps to repair spalled concrete are.
Remove the loose and damaged concrete.
Use a wire brush to loosen weak areas.
Pitting in a concrete floor spalling and pitting repair step 2.
Learn more about fi.
Before patching the area apply a bonding agent to the affected surface to ensure proper adhesion.
Concreteresurfacing fixspalledconcrete howtorepairconcrete in this video i m showing you how to resurface a spalled concrete patio.
Clean the concrete by pressure washing or grinding it.
Patch the deep areas 1 8 or more with the resurfacing material first and let dry.
Get rid of concrete spalling by resurfacing the concrete if your driveway surface has spalling concrete the most likely cause is an installation mistake.